Description and Applications |
|
HJ350R is a
titanium type electrode with excellent mechanical
properties and weld ability. Deposited metal hardness of
as welded is about HV 300~350. Restricting is good and
slag is easy to remove. |
|
|
|
Guideline in Usage |
|
1. |
Electrode should be re-dried
at 100~200℃
for 60 minutes before use. |
|
2. |
Remove dirt such
as oil and dust from groove. |
|
|
|
|
|
|
Typical
Chemical Composition of Weld Metal(%) |
|
C |
Si |
Mn |
P |
S |
Cr |
Mo |
|
0.110 |
0.390 |
0.620 |
0.010 |
0.010 |
2.20 |
0.661 |
|
|
|
|
Typical Hardness of
Weld Metal (Vickers Hardness) |
|
|
|
|
|
Size & Recommended Current Range(AC
) |
|
|
|
3.2 |
4.0 |
5.0 |
|
|
350 |
350/400 |
450 |
|
Current (Amp) |
F |
100~140 |
140~190 |
180~230 |
|
|
|
|
 |