Description and Applications |
HE310 is a lime-Titania
type electrode. Deposited metal contains about 25% Cr
and 20% Ni. Mechanical properties are excellent. It
provides good corrosion resistance and heat resistance
in as-welded condition.
Welding of stainless
steel 310, Cr-Mo steel, 13Cr steel. |
|
Guideline in Usage |
1. |
Electrodes should be re-dried at
250
~
300℃ for one hour before use. |
2. |
Keep arc and
amperage as short and low as possible. Remove
dirt such as oil and dust from the groove. |
3. |
Sufficient crater
treatment is required since deposited metal is a
completely austenitic structure and crack
resistance is slightly low. |
4. |
Keep the
interpass temperature under 150℃. |
|
|
|
Typical
Chemical Composition of Weld Metal(%) |
C |
Si |
Mn |
P |
S |
Ni |
Cr |
Mo |
0.100 |
0.550 |
1.22 |
0.023 |
0.003 |
20.50 |
26.90 |
0.560 |
|
|
Typical Mechanical Properties of Weld Metal |
Yield Strength
N/mm2 |
Elongation
% |
598 |
38 |
|
|
Size & Recommended Current Range(AC
) |
|
2.6 |
3.2 |
4.0 |
5.0 |
|
300 |
350 |
350 |
350 |
Current (Amp) |
F |
60~85 |
85~120 |
115~150 |
150~200 |
V,OH |
50~75 |
75~105 |
95~120 |
|
|
|
|