Description and Applications |
Welding of 18-8 austenitic stainless steels for chemical
apparatus, containers and plants. Slag is easy to
detach and arc is stable, less spatter loss and bead
appearance is beautiful |
|
Guideline in Usage |
1. |
Electrodes should be re-dried at
250
~
300℃ for one hour before use |
2. |
Excessively
wide weaving may cause welding defects. Keep
weaving width to less than 2.5 times electrode
diameter. |
3. |
Remove dirt such
as oil and dust from the groove. |
|
|
|
|
Welding
Parameters |
SIZE |
2.0mm |
2.6mm |
3.2mm |
4.0mm |
5.0mm |
Length |
250mm |
300mm |
350mm |
350mm |
350mm |
Current (Amp) |
F, Fillet |
30-50 |
60-85 |
85-120 |
115-150 |
150-190 |
V, OH |
30-50 |
50-70 |
75-105 |
95-130 |
|
|
|
Typical Mechanical Properties |
Tensile Strength |
590 N/mm2 |
Elongation |
43
% |
|
|
Typical Chemistry
(wt%) |
Carbon |
0.05 |
Silicon |
0.80 |
Manganese
|
0.77 |
Chromium |
19.1 |
Nickel |
9.7
|
Molybdenum |
0.11 |
Sulphur |
0.006 |
Phosphorus |
0.01 |
Iron |
Bal |
|
|
|